ESDU FAT E0506 A 1977-APR-01 Endurance of bonded lap jonts Alumnum alloy sheet materal phenolc resnvnyl powder glue tensle loadng

More details

Download

PDF AVAILABLE FORMATS IMMEDIATE DOWNLOAD
$162.50 tax incl.

$325.00 tax incl.

(price reduced by 50 %)

1000 items in stock

ESDU Fat E.05.06 presents curves of alternating stress against endurance obtained from an analysis of 280 constant amplitude room temperature tests of joints with adherends 0.033 to 0.082 in (0.08 to 2 mm) thick (t) glued over a length (l) of 0.375 to 1.96 in (10 to 50 mm). The stress ratio lay between zero and 0.22. The clad sheet material was either naturally-aged Al-Cu-Mg 2024-T3 or artificially-aged Al-Zn-Mg 7075-T6. Four sets of mean endurance curves are given for failure in the glue, each set for one value of adherend thickness and a range of values of l/t. However, for two adherend thicknesses, sets of curves are also included for failure in the adherend. The average shear stress in the glue for a given tensile stress in the adherends and l/t may also be read off the curves. A worked example illustrates the use of the data.

Contact us